I made a ageing solution from chemicals found in my gararge.... This is the same ring after one treatment.. Took all of 5 min. total... It can be dipped again and again for a more aged, ground dug effect.. You can even put a drop of battery acid on it and it'd look like one of the Stalingrad rings.. *Be suspicious of ANY ground dug ring: